Außendurchmesser Zoll Ave. Wall Zoll Mindeststreckgrenze (PSI) Min. Zugfestigkeit (PSI) Theoretischer Berstdruck * (PSI) Arbeitsdruck (PSI) 25 % des Berstdrucks Theoretische Fließgrenze ** (PSI) Kollapsdruck *** (PSI)
0.250 0.020 30,000 75,000 14,286 3,571 5,714 4,416
0.250 0.028 30,000 75,000 21,649 5,412 8,660 5,967
0.250 0.035 30,000 75,000 29,167 7,292 11,667 7,224
0.250 0.049 30,000 75,000 48,355 12,089 19,342 9,455
0.250 0.065 30,000 75,000 81,250 20,313 32,500 11,544
0.375 0.020 30,000 75,000 8,955 2,239 3,582 3,029
0.375 0.028 30,000 75,000 13,166 3,292 5,266 4,145
0.375 0.035 30,000 75,000 17,213 4,303 6,885 5,077
0.375 0.049 30,000 75,000 26,534 6,634 10,614 6,816
0.375 0.065 30,000 75,000 39,796 9,949 15,918 8,597
0.500 0.020 30,000 75,000 6,522 1,630 2,609 2,201
0.500 0.028 30,000 75,000 9,459 2,365 3,784 3,172
0.500 0.035 30,000 75,000 12,209 3,052 4,884 3,906
0.500 0.049 30,000 75,000 18,284 4,571 7,313 5,201
0.500 0.065 30,000 75,000 26,351 6,588 10,541 6,786
0.500 0.083 30,000 75,000 37,275 9,319 14,910 8,307
0.625 0.020 30,000 75,000 5,128 1,282 2,051 1,859
0.625 0.028 30,000 75,000 7,381 1,845 2,953 2,568
0.625 0.035 30,000 75,000 9,459 2,365 3,784 3,172
0.625 0.049 30,000 75,000 13,947 3,487 5,579 4,335
0.625 0.065 30,000 75,000 19,697 4,924 7,879 5,591
0.625 0.083 30,000 75,000 27,124 6,781 10,850 6,910
0.625 0.095 30,000 75,000 32,759 8,190 13,103 7,734
0.625 0.109 30,000 75,000 40,172 10,043 16,069 8,639
0.750 0.028 30,000 75,000 6,052 1,513 2,421 2,156
0.750 0.035 30,000 75,000 7,721 1,930 3,088 2,669
0.750 0.049 30,000 75,000 11,273 2,818 4,509 3,664
0.750 0.065 30,000 75,000 15,726 3,931 6,290 4,749
0.750 0.083 30,000 75,000 21,318 5,330 8,527 5,905
0.750 0.095 30,000 75,000 25,446 6,362 10,179 6,637
0.750 0.109 30,000 75,000 30,733 7,683 12,293 7,453
0.750 0.120 30,000 75,000 35,294 8,824 14,118 8,064
0.875 0.020 30,000 75,000 3,593 898 1,437 1,340
0.875 0.028 30,000 75,000 5,128 1,282 2,051 1,859
0.875 0.035 30,000 75,000 6,522 1,630 2,609 2,201
0.875 0.049 30,000 75,000 9,459 2,365 3,784 3,172
0.875 0.065 30,000 75,000 13,087 3,272 5,235 4,126
0.875 0.083 30,000 75,000 17,560 4,390 7,024 5,152
0.875 0.095 30,000 75,000 20,803 5,201 8,321 5,807
0.875 0.109 30,000 75,000 24,886 6,221 9,954 6,543
0.875 0.120 30,000 75,000 28,346 7,087 11,339 7,100
1.000 0.028 30,000 75,000 4,449 1,112 1,780 1,633
1.000 0.035 30,000 75,000 5,645 1,411 2,258 2,027
1.000 0.049 30,000 75,000 8,149 2,037 3,259 2,796
1.000 0.065 30,000 75,000 11,207 2,802 4,483 3,647
1.000 0.083 30,000 75,000 14,928 3,732 5,971 4,567
1.000 0.095 30,000 75,000 17,593 4,398 7,037 5,159
1.000 0.109 30,000 75,000 20,908 5,227 8,363 5,827
1.000 0.120 30,000 75,000 23,684 5,921 9,474 6,336
1.000 0.134 30,000 75,000 27,459 6,865 10,984 6,963
1.250 0.035 30,000 75,000 4,449 1,112 1,780 1,633
1.250 0.049 30,000 75,000 6,380 1,595 2,552 2,260
1.250 0.065 30,000 75,000 8,705 2,176 3,482 2,958
1.250 0.083 30,000 75,000 11,485 2,871 4,594 3,719
1.250 0.095 30,000 75,000 13,443 3,361 5,377 4,213
1.250 0.109 30,000 75,000 15,843 3,961 6,337 4,776
1.250 0.120 30,000 75,000 17,822 4,455 7,129 5,207
1.250 0.134 30,000 75,000 20,468 5,117 8,187 5,742
1.500 0.035 30,000 75,000 3,671 918 1,469 1,367
1.500 0.049 30,000 75,000 5,243 1,311 2,097 1,896
1.500 0.065 30,000 75,000 7,117 1,779 2,847 2,487
1.500 0.083 30,000 75,000 9,333 2,333 3,733 3,136
1.500 0.095 30,000 75,000 10,878 2,719 4,351 3,559
1.500 0.109 30,000 75,000 12,754 3,188 5,101 4,043
1.500 0.120 30,000 75,000 14,286 3,571 5,714 4,416
1.500 0.134 30,000 75,000 16,315 4,079 6,526 4,881
1.500 0.148 30,000 75,000 18,439 4,610 7,375 5,336
1.750 0.035 30,000 75,000 3,125 781 1,250 1,176
1.750 0.049 30,000 75,000 3,864 966 1,546 1,434
1.750 0.065 30,000 75,000 6,019 1,505 2,407 2,146
1.750 0.083 30,000 75,000 7,860 1,965 3,144 2,711
1.750 0.095 30,000 75,000 9,135 2,284 3,654 3,080
1.750 0.109 30,000 75,000 10,672 2,668 4,213 3,504
1.750 0.120 30,000 75,000 11,921 2,980 4,768 3,832
1.750 0.134 30,000 75,000 13,563 3,391 5,425 4,242
1.750 0.148 30,000 75,000 15,268 3,817 6,107 4,645
1.750 0.165 30,000 75,000 17,430 4,357 6,972 5,124
2.000 0.035 30,000 75,000 2,720 680 1,088 1,032
2.000 0.049 30,000 75,000 3,864 966 1,546 1,434
2.000 0.065 30,000 75,000 5,214 1,303 2,086 1,887
2.000 0.083 30,000 75,000 6,788 1,697 2,715 2,387
2.000 0.095 30,000 75,000 7,873 1,968 3,149 2,715
2.000 0.109 30,000 75,000 9,175 2,294 3,670 3,092
2.000 0.120 30,000 75,000 10,227 2,557 4,091 3,384
2.000 0.134 30,000 75,000 11,605 2,901 4,642 3,751
2.000 0.148 30,000 75,000 13,028 3,257 5,211 4,111
2.000 0.165 30,000 75,000 14,820 3,705 5,928 4,542